Ingen varer
Priserne er inklusiv moms
PrimaCreator Value Flex Resin er en prisvenlig harpiks fremstillet af de bedste råmaterialer. Den giver dig 3D-udskrifter af god kvalitet. Hærd dine 3D-udskrifter i sollys eller i et UV-hærdekammer. Når hærdningen er færdig, får du fleksible 3D-udskrifter med meget lille krympning. Objekterne har et meget blødt touch.
De vigtigste fordele ved PrimaCreator Value Flex Resin:
På Fjernlager
Advarsel: Sidste enheder på lager!
Tilgængelighedsdato:
24598
When you want astonishing results for less cost than many other brands - PrimaCreator VALUE resin should be your first choice!
Resin from our VALUE line is a high-quality resin made from the best materials.
Your prints cures in sunlight or a UV curing chamber. When the curing is finished, the result is a flexible print with very small shrinkage and very soft to the touch.
The finished print is a solid color part with a beautiful matte surface with excellent details and smooth layer transitions.
Flexible resin is the perfect resin when you are looking for high detail results that needs to have a very high impact strength. The shore hardness of 65-75 D together with an incredible elongation at break of 130% makes it a resin that can use in many applications and areas.
VALUE resin is developed to perform well on low powered DLP machines such as the Wanhao Duplicator 7, SparkMaker Anycubic Photon, Zortrax Inkspire and other printers that uses UV light for curing.
Optimized for UV Lightsource 395 – 405 nm.
Fast curing time, 4 – 12 (depending on color) seconds per layer for quicker prints.
After printing, clean you print in IPA (Isopropyl Alcohol) to rinse of extra resin left on the model.
When it´s time for curing you can use sunlight or a uv curing chamber.
Depending on print the curing times can vary:
Mærke | Prima Creator |
Materiale | FLEX |
Farve | Hudfarvet |
Volumen | 500ml |
Lager | Online |
Bølgelængde | 405nm |
Flexural modulus | 1.882 - 2.385 MPa |
Flexural strength | 40-70 MPa |
Hot deformation temp. | 80 ℃ |
Thermal expansion | 95*E-6 |
Volume shrinkage | 3.72 - 4.24% |
Linear shrinkage | 1.05 - 1.35% |
Tensile strength | 30 - 52 MPa |
Tensile modulus | 1.779 - 2.385 MPa |
Elongation at break | 130% |
Hardness (Shore D) | 65 - 75D |
Glass transition temp. | 100 ℃ |
Density | 1.05-1.25g/cm3 |
Notched impact strength | 41-48 j/m |
Viscosity | 150-300 MPa·s |
Curing time | 4 - 12s for layer thickness 0.05 mm Bottom layer 40 - 60 s |