The following parameters are only suggested print settings for this material. To ensure the best print quality, it is necessary to choose the appropriate settings for a specific printer and printing conditions.
Mærke | Fiberlogy |
Materiale | PLA |
Diameter tolerance | +/- 0,02 mm |
Print temperatur | 200°C - 230°C |
Opvarmet seng krævet | Ja |
Anbefalet temperatur på seng | 50°C - 70°C |
Kompatibel - Bambu Lab AMS | Nej |
Nozzle Temperature | 200-230°C |
Bed Temperature | 50°C |
Closed chamber | not required |
Fan | 75-100% |
Flowrate | 95-105% |
Printing Speed | <60 mm/s |
Surface | PEI, glass, masking tape |
Retraction (direct) | 2-3 mm |
Retraction (bowden) | 4-6 mm |
Retraction Speed | 20-45 mm/s |
Drying conditions | 40°C / 4h |
Notes | Due to the strong adhesion, damage to the bed surface (eg PEI) may occur. We recommend printing on a tape. |